Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PB320G6 Nylon 6, 30% Glass Fiber, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB320G6 Nylon 6, 30% Glass Fiber, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
DIN 53479
Water Absorption 4.8 %
4.8 %
DIN 53495
Moisture Absorption at Equilibrium 1.6 %
1.6 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM-D785
Tensile Strength, Yield 110 MPa
16000 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 170 MPa
24700 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM-D790
Izod Impact, Notched 0.900 J/cm

@Temperature 23.0 °C
1.69 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
>= 200 °C
>= 392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
DIN 53461
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DIN 53482
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
DIN 53482
Dielectric Constant 4.3

@Frequency 1e+6 Hz
4.3

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 65.0 kV/mm
1650 kV/in
VDE 0303/4
Users viewing this material also viewed the following: