Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram Polytron P35B03 Copolymer Polypropylene, Chemically Coupled 35% Long Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P35B03 Copolymer Polypropylene, Chemically Coupled 35% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A CHEMICALLY COUPLED 35% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM-D792
Linear Mold Shrinkage 0.0014 cm/cm
0.0014 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Tensile Modulus 7.00 GPa
1020 ksi
ASTM-D790
Flexural Strength 160 MPa
23200 psi
ASTM-D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM-D790
Izod Impact, Notched 1.60 J/cm

@Temperature 23.0 °C
3.00 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ASTM-D648
Users viewing this material also viewed the following: