Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.00 GPa | 1020 ksi | |
Plastcom SLOVAMID 66/6 GF 20 PA66/6, 20% glass fibre FeaturesChemically reinforced alloy PA 66 and PA 6 with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Nilit FRIANYL A63 H-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Nilit FRIANYL B63 GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued * The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | |
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | |
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Polyram PlusTek PB300G4 Nylon 6 for Injection Molding, 20% Glass-Fiber Reinforced 20% Glass fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ASTM-D790 |
Polyram Polytron P35B03 Copolymer Polypropylene, Chemically Coupled 35% Long Glass Fiber A CHEMICALLY COUPLED 35% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 230 S PBT-GF15 FR(17) 15% Glass Reinforced, Flame Retardant |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecomid® NB40 GR20 NL PA 6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BGK-30 X PA6-(GF+GB)30 Information provided by EMS Grivory |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecotek® PC30 GR20 GR003 ZG20 PC, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 7035 Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Modulus | 7.00 GPa @Temperature 70.0 °C, Time 1.44e+6 sec |
1020 ksi @Temperature 158 °F, Time 400 hour |
62% RH |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |