Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A chemically coupled 50% long glass fiber reinforced natural polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 135 MPa
19600 psi
ISO 527
Elongation at Break 1.7 %
1.7 %
ISO 527
Tensile Modulus 12.9 GPa
1870 ksi
ISO 527
Flexural Strength 210 MPa
30500 psi
ISO 178
Flexural Modulus 11.0 GPa
1600 ksi
ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
ISO 180
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
ISO 179
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: