Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.31 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
Plastcom SLOVASTER® B1 BT PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792, ISO 1183
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1005 Resin.
Density 1.31 g/cc
0.0473 lb/in³
±0.03 g/cm³; DIN 53479
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® S600F20 BK851 PBT  (Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® S600F20 NC010 PBT  (Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Nilit FRIANYL A63 H-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.31 g/cc
0.0473 lb/in³
DIN 53479; ASTM D792
Kolon SPESIN® KP211 General Purpose PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
Density 1.31 g/cc
0.0473 lb/in³
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Techmer ES Elastoblend® PA6/6 GF30 IM2 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Techmer ES Electrafil® PC-50/EC/VO Polycarbonate, Conductive Carbon Filled
Conductive Carbon, Powder Modified with Flame Retardant
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66
LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact.
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.31 g/cc
0.0473 lb/in³
DIN 53479
Polyram RamTough RZ309G18 Polycarbonate, 18% Glass Fiber
18% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.31 g/cc
0.0473 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66
Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded
BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded
Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural
Information provided by Eurotec®
Copyright © lookpolymers.com All Rights Reserved