Material Notes:
A chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 140 MPa
20300 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 13.0 GPa
1890 ksi
ISO 527
Flexural Strength 230 MPa
33400 psi
ISO 178
Flexural Modulus 14.5 GPa
2100 ksi
ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179
2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: