Precision Polymer Engineering C40M Chloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering C40M Chloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chloroprene elastomer, 36-45 °IRHD. Formulated to BS 2752 grade C40.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
°IRHD; ASTM D1415
44
44
°IRHD, +6 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 12.68 MPa
1839 psi
-0.5% change after 168 hours @ 70°C; ASTM D412
12.74 MPa
1848 psi
ASTM D412
Elongation at Break 476.19 %
476.19 %
-1% change after 168 hours @ 70°C; ASTM D412
481 %
481 %
ASTM D412
Compression Set 33 %
33 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 260 °C
>= 500 °F