Material Notes:
Self-lubricating, Nitrile Rubber, 75-85 °IRHD. Copolymer of acrylonitrile and butadiene. Special filler incorporated to enhance operation in dynamic sealing applications. ASTM & ISO designation = NBR.Applications: Excellent resistance to petroleum based oils and fuels. Good compression set, tear and abrasion resistance. Specially compounded for use in dynamic sealing applications requiring a low surface co-efficient of friction.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
95
95
°IRHD, +15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 11.2 MPa
1620 psi
-20% change after 70 hours @ 100°C; ASTM D412
14.0 MPa
2030 psi
ASTM D412
Elongation at Break 75.0 %
75.0 %
-40% change after 70 hours @ 100°C; ASTM D412
125 %
125 %
ASTM D412
Compression Set 25 %
25 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F