Material Notes:
Isoflow Graphite Rings facilitate an even flow of oil around the circumference of the billet. This even flow results in improved billet surface quality over long casting campaigns. Isoflow Graphite Rings are fabricated using high strength iso-statically pressed graphite that features very uniform pore size and pore distribution.Average Grain Size: 15 micronsAdvantagesISO 9002 Certified Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.70 - 1.75 g/cc
0.0614 - 0.0632 lb/in³
Open Porosity 15 %
15 %
Permeability 0.0030
0.0030
Darcys
Mechanical Properties Metric English Comments
Modulus of Elasticity 10.5 - 11.2 GPa
1520 - 1620 ksi
Flexural Strength 45.0 - 46.5 MPa
6530 - 6740 psi
Compressive Strength 89.7 - 91.4 MPa
13000 - 13300 psi
Users viewing this material also viewed the following: