Mechanical Properties Metric English Comments
Flexural Strength 45.0 - 46.5 MPa
6530 - 6740 psi
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Isoflow Graphite Rings facilitate an even flow of oil around the circumference of the billet. This even flow results in improved billet surface quality over long casting campaigns. Isoflow Graphit..