Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVALEN PH 52 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVAMID 66 SHI PA66, improved strength Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Flexural Strength | 45.0 - 60.0 MPa | 6530 - 8700 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co.. |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 45.0 - 47.0 MPa @Temperature 23.0 °C |
6530 - 6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 45.0 MPa @Temperature 1500 °C |
6530 psi @Temperature 2730 °F |
|
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | 3.5%; ISO 178 |
GEHR Plastics POM-ESD Acetal, Antistatic Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-722 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Flexural Strength | 45.0 - 47.0 MPa | 6530 - 6820 psi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX98501 PE LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | GB/9341 |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | UNI EN ISO 14125: 2000 |
CRP Technology Windform® FX Polyamide Composite Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T10L Talc Reinforced |
|||
Flexural Strength | 45.0 MPa @Temperature 65.0 °C |
6530 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M30L Mica Reinforced |
|||
Flexural Strength | 45.0 MPa | 6530 psi | STN EN ISO 178 |
Plastcom SLOVALEN PH 51 T 15 Polypropylene Homopolymer, 15% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 15% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Teknor Apex Sinpolene CPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene