Material Notes:
Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation provides a product with an outstanding combination of high compressive strength and low thermal conductivity. Incombustible, Isomag® 175 is totally free of asbestos and may be cut or machined with readily available tools.ApplicationsPlaten press insulation Arc chutes Resistor grids Induction furnaces Pot pads Buss support insulation Foundry bottom boards Blow boards AdvantagesLow heat loss at higher temperatures Low shrinkage at temperature use limit High temperature rating Asbestos and ceramic fiber free Information provided by Pyrotek.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
Density 1.54 g/cc
0.0556 lb/in³
Water Absorption <= 0.50 %
<= 0.50 %
with silicone treatment
25 %
25 %
Open Porosity 44.1 %
44.1 %
Mechanical Properties Metric English Comments
Flexural Strength 27.6 MPa
4000 psi
Compressive Strength 37.9 MPa
5500 psi
27.0 MPa

@Strain 5.00 %,
Temperature 500 °C
3920 psi

@Strain 5.00 %,
Temperature 932 °F
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
Thermal Properties Metric English Comments
Thermal Conductivity 0.270 W/m-K

@Temperature 195 °C
1.87 BTU-in/hr-ft²-°F

@Temperature 383 °F
0.280 W/m-K

@Temperature 315 °C
1.94 BTU-in/hr-ft²-°F

@Temperature 599 °F
0.340 W/m-K

@Temperature 600 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Continuous use
1050 °C
1920 °F
Flammability, UL94 V-0
V-0
V-0
Shrinkage 1.50 %

@Temperature 1000 °C
1.50 %

@Temperature 1830 °F
Linear
4.30 %

@Temperature 1000 °C
4.30 %

@Temperature 1830 °F
Thickness
Electrical Properties Metric English Comments
Volume Resistivity 6.90e+14 ohm-cm
6.90e+14 ohm-cm
Dielectric Constant 4.1

@Frequency 1000 Hz
4.1

@Frequency 1000 Hz
Dielectric Strength 9.80 kV/mm
249 kV/in
Dielectric Breakdown 28100 V
28100 V
Dissipation Factor 0.050
0.050
Arc Resistance 292 sec
292 sec