Material Notes:
MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: Troughs Filter bowls Furnace linings Transfer crucibles Door insulation AdvantagesLow thermal conductivity Reduces warping of vessels and troughing Promotes greater temperature control Minimizes heat transfer Can be designed to be reused Minimizes hot face temperature of vessels Provides low shrinkage at high temperatures Not wet by molten aluminum Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.288 - 0.352 g/cc
0.0104 - 0.0127 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 1.10 MPa
160 psi
to 30% deformation with density of 0.288 g/cc
1.70 MPa
247 psi
to 30% deformation with density of 0.320 g/cc
3.40 MPa
493 psi
to 30% deformation with density of 0.352 g/cc
Thermal Properties Metric English Comments
Thermal Conductivity 0.0290 W/m-K

@Temperature 260 °C
0.201 BTU-in/hr-ft²-°F

@Temperature 500 °F
(Standard and Hydrophobic)
0.0420 W/m-K

@Temperature 537 °C
0.291 BTU-in/hr-ft²-°F

@Temperature 999 °F
Standard
0.0480 W/m-K

@Temperature 537 °C
0.333 BTU-in/hr-ft²-°F

@Temperature 999 °F
(Hydrophobic)
0.0490 W/m-K

@Temperature 649 °C
0.340 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Standard
0.0560 W/m-K

@Temperature 649 °C
0.389 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Hydrophobic
Maximum Service Temperature, Air 1000 °C
1830 °F
Continuous
Shrinkage 0.300 %

@Temperature 538 °C,
Time 86400 sec
0.300 %

@Temperature 1000 °F,
Time 24.0 hour
0.600 %

@Temperature 815 °C,
Time 86400 sec
0.600 %

@Temperature 1500 °F,
Time 24.0 hour
1.00 %

@Temperature 954 °C,
Time 86400 sec
1.00 %

@Temperature 1750 °F,
Time 24.0 hour