Thermal Properties Metric English Comments
Thermal Conductivity 0.0560 W/m-K

@Temperature 649 °C
0.389 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Hydrophobic
Pyrotek MT-29P Microporous Panel Insulation
MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel.Applica..
Thermal Conductivity 0.0560 W/m-K

@Temperature 649 °C
0.389 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Hydrophobic
Pyrotek MT-29Q Quilted Microporous Insulation
MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains ..
Thermal Conductivity 0.0560 W/m-K

@Temperature 649 °C
0.389 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Hydrophobic
Pyrotek MT-29L Microporous Ladle Lining Insulation
MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac..
Thermal Conductivity 0.0560 W/m-K

@Temperature 649 °C
0.389 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Hydrophobic
Pyrotek MT-29B Microporous Insulating Board
MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T..