Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0290 W/m-K @Temperature 260 °C |
0.201 BTU-in/hr-ft²-°F @Temperature 500 °F |
(Standard and Hydrophobic) |
Pyrotek MT-29P Microporous Panel Insulation MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel.Applica.. |
|||
Thermal Conductivity | 0.0290 W/m-K @Temperature 260 °C |
0.201 BTU-in/hr-ft²-°F @Temperature 500 °F |
(Standard and Hydrophobic) |
Pyrotek MT-29Q Quilted Microporous Insulation MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains .. |
|||
Thermal Conductivity | 0.0290 W/m-K @Temperature 260 °C |
0.201 BTU-in/hr-ft²-°F @Temperature 500 °F |
(Standard and Hydrophobic) |
Pyrotek MT-29L Microporous Ladle Lining Insulation MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac.. |
|||
Thermal Conductivity | 0.0290 W/m-K @Temperature 260 °C |
0.201 BTU-in/hr-ft²-°F @Temperature 500 °F |
(Standard and Hydrophobic) |
Pyrotek MT-29B Microporous Insulating Board MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T.. |