Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Pyrocast ALF2 Low Cement Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast ALF2 Low Cement Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and holding furnace linings Ladles Launders Degassing boxes De-mag boxes AdvantagesOutstanding hot strength High abrasion resistance Resistant to molten aluminum attack Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.595 g/cc
0.09375 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0441 GPa

@Temperature 816 °C
6.40 ksi

@Temperature 1500 °F
Hot
0.0200 GPa

@Treatment Temp. 110 °C
2.90 ksi

@Treatment Temp. 230 °F
fired and cooled
0.0300 GPa

@Treatment Temp. 954 °C
4.35 ksi

@Treatment Temp. 1750 °F
fired and cooled
Thermal Properties Metric English Comments
Thermal Conductivity 1.56 W/m-K

@Temperature 260 °C
10.8 BTU-in/hr-ft²-°F

@Temperature 500 °F
1.59 W/m-K

@Temperature 538 °C
11.0 BTU-in/hr-ft²-°F

@Temperature 1000 °F
1.69 W/m-K

@Temperature 816 °C
11.7 BTU-in/hr-ft²-°F

@Temperature 1500 °F
1.83 W/m-K

@Temperature 1093 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Maximum Service Temperature, Air 1704 °C
3099 °F
Shrinkage 0.100 %

@Temperature 954 °C
0.100 %

@Temperature 1750 °F
Linear
Component Elements Properties Metric English Comments
Al2O3 61.34 %
61.34 %
Alkalis 0.22 %
0.22 %
CaO 1.92 %
1.92 %
Fe2O3 0.98 %
0.98 %
MgO 0.11 %
0.11 %
SiO2 32.86 %
32.86 %
TiO2 1.43 %
1.43 %
Users viewing this material also viewed the following: