Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0200 GPa @Treatment Temp. 110 °C |
2.90 ksi @Treatment Temp. 230 °F |
fired and cooled |
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol.. |
|||
Modulus of Rupture | 0.0200 GPa @Treatment Temp. 110 °C |
2.90 ksi @Treatment Temp. 230 °F |
fired and cooled |
Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable Pyrocast AL3 is suited for use in aluminum melting equipment and metal transfer areas where sever wear or alkali attack are a factor. Pyrocast AL3 is a high-purity mullite based refractory with low.. |
|||
Modulus of Rupture | 0.0200 GPa @Treatment Temp. 110 °C |
2.90 ksi @Treatment Temp. 230 °F |
fired and cooled |
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an.. |