Mechanical Properties Metric English Comments
Modulus of Rupture 0.0200 GPa

@Treatment Temp. 110 °C
2.90 ksi

@Treatment Temp. 230 °F
fired and cooled
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable
Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol..
Modulus of Rupture 0.0200 GPa

@Treatment Temp. 110 °C
2.90 ksi

@Treatment Temp. 230 °F
fired and cooled
Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable
Pyrocast AL3 is suited for use in aluminum melting equipment and metal transfer areas where sever wear or alkali attack are a factor. Pyrocast AL3 is a high-purity mullite based refractory with low..
Modulus of Rupture 0.0200 GPa

@Treatment Temp. 110 °C
2.90 ksi

@Treatment Temp. 230 °F
fired and cooled
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable
Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an..