Pyrotek Pyromat TS-045 Electrical Insulating Board

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Pyrotek, Inc.
Trade Name Pyromat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyromat TS-045 Electrical Insulating Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyromat TS-045 is a black laminate, press molded from high-temperature thermoset resin and reinforced with glass filament mat. Its composition ensures excellent chemically resistance and antistatic properties. Each board is surface ground to achieve accurate dimensions on thickness and parallelism. Pyromat TS-045 is specifically formulated to provide optimum properties for the manufacture of solder pallets for the PCB industry.ApplicationsWave solder pallet / carrier support AdvantagesSuperior antistatic properties Excellent chemical durability Exceptional thermal resistance Superior parallelism and flatness Good machining characteristics Easy to wash and handle Dimensionally stable Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.80 - 1.90 g/cc
0.0650 - 0.0686 lb/in³
Water Absorption <= 0.18 %
<= 0.18 %
Mechanical Properties Metric English Comments
Flexural Strength 400 MPa
58000 psi
Compressive Strength 500 MPa
72500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Continuous
300 °C
572 °F
Intermittent
Electrical Properties Metric English Comments
Surface Resistance 1.00e+6 - 1.00e+10 ohm
1.00e+6 - 1.00e+10 ohm