Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 400 MPa | 58000 psi | |
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
PolyOne OnForce™ LFT AM-30LCF/001 Grey Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D790 |
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures... |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D-790 |
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D 790 |
RTP Company RTP 4085 SI 2 Polyphthalamide (PPA), Carbon Fiber - Silicone Lubricated |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Nilit FRIANYL A63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D 790 |
RTP Company VLF 80209 EM HS Nylon 6/6 (PA), Long Glass Fiber - Easy Molding - Heat Stabilized |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Flexural Strength | 400 MPa | 58000 psi | |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 400 MPa | 58000 psi | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Flexural Strength | 400 MPa | 58000 psi | |
Sapco Si.SiC Silicon Carbide Information provided by Sapco. |
|||
Flexural Strength | 400 MPa | 58000 psi | Bending Strength; Dual Ring Method (0.63 mm Substrate Thickness); DIN 52292 |
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D790 |
Chase Plastics CP Pryme® NNN260L (Dry) Nylon 66/6 Copolymer, 60% Glass Fiber Reinforced Features: Good chemical resistanceGood compressive strengthGood creep resistanceGood dimensional stabilityGood flowGrease resistantOil resistantHigh rigiditySolvent resistantHigh tensile strengthHig.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass 60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram. |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D790 |
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM-F394 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM F417 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | 400 MPa | 58000 psi | Typical for SiC |
Destech Silicon Carbide, Solid or Foamed Destech silicon carbide foam is produced by chemical vapor reaction (CVR), in which high temperature silicon bearing gases convert glassy, or vitreous, carbon foam to SiC. Destech SiC foam has no c.. |
|||
Flexural Strength | >= 400 MPa | >= 58000 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe. |
|||
Flexural Strength | 400 MPa | 58000 psi | crosswise; IPC TM-650 2.4.4 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Flexural Strength | 400 MPa | 58000 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Celanese Celstran® PA66-GF50-20 AD3007 Nylon 66, 50% Glass Reinforced Material code according to ISO 1043-1: PA66Information provided by Celanese |
|||
Flexural Strength | 400 MPa | 58000 psi | ISO 178 |
Celanese Celstran® PA6-GF60-03 PA6, 60% Glass Reinforced 60% long fiber glass reinforced, heat stabilized, Nylon 660% long fiber glass reinforced, heat stabillized, Nylon 6Information provided by Celanese |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D 790 |
RTP Company RTP 2287 HF Polyetheretherketone (PEEK), Carbon Fiber - High Flow |
|||
Flexural Strength | 400 MPa | 58000 psi | ASTM D 790 |
RTP Company RTP 4085 TFE 10 Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated |
|||
Flexural Strength | 400 MPa | 58000 psi | |
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |