Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Qualchem Danamid FE Polyamide 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid FE Polyamide 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard type polyamide with good flowing propertiesInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
50 mm/min; ISO 527-1,2
Elongation at Yield 4.0 %
4.0 %
ISO 527-1,2
Tensile Modulus 2.50 GPa
363 ksi
ISO 527-1,2
Charpy Impact Unnotched NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
DIN 53453
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Comparative Tracking Index 600 V
600 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 3.0 - 3.5 %
3.0 - 3.5 %
DIN 53714