Impact resistant, dryInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
DIN 53479
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527-1,2
Elongation at Yield 10 %
10 %
ISO 527-1,2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-1,2
Charpy Impact Unnotched NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
DIN 53453
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched >= 0.500 J/cm²

@Temperature -20.0 °C
>= 2.38 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
>= 1.20 J/cm²

@Temperature 23.0 °C
>= 5.71 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Comparative Tracking Index 600 V
600 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 3.0 - 3.2 %
3.0 - 3.2 %
DIN 53714