Material Notes:
Filled with mineralsInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
DIN 53479
Filler Content 23 - 27 %
23 - 27 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
50 mm/min; ISO 527-1,2
Tensile Modulus 3.40 GPa
493 ksi
ISO 527-1,2
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Comparative Tracking Index 500 V
500 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
DIN 53714
Users viewing this material also viewed the following: