Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 500 V | 500 V | IEC 112 |
Qualchem Danamid FEW-25 Polyamide 6, 25% Mineral Filled Filled with mineralsInformation provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 112 |
Qualchem Danamid FGFS-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Impact modified.Information provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Average value: 583 V Grade Count:6 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Average value: 592 V Grade Count:12 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
DSM Akulon® K224-TPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)
(discontinued **)&l The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
DSM Akulon® Ultraflow™ K-FHGM24 Nylon 6-30% Glass and Mineral Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
Comparative Tracking Index | 500 V | 500 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Comparative Tracking Index | 500 V | 500 V | TS EN 60112 |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Comparative Tracking Index | 500 V | 500 V | TS EN 60112 |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
DSM Akulon® K224-HG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Comparative Tracking Index | 500 V | 500 V | DIN IEC 112 / VDE 030 t1 |
DSM Fibre Intermediates Nyrim® 2000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Comparative Tracking Index | 500 V | 500 V | DAM; IEC 60112 |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurotec® Tecomid® NB40 GR20 NL PA 6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V @Thickness 3.00 mm |
500 V @Thickness 0.118 in |
IEC 60112; IEC/EN 60893-2 6.4 |
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T.. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecoform® PO20 AR10 NL HS POM, 10% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 112 |
LATI LARAMID G/45 45% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |