Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for applications subject to impacts and rough handling. QC-8704 is also suggested for applications requiring excellent fatigue resistance. It incorporates short glass fibers for easy flow. Form and Color = Rolled Sheet, Black. Glass Fiber Length = .25 inch.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.35 %
0.35 %
24 Hrs. ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 65
65
ASTM D2583
Tensile Strength, Ultimate 275 MPa
39900 psi
ASTM D638
Flexural Yield Strength 413 MPa
59900 psi
ASTM D790
Flexural Modulus 17.2 GPa
2490 ksi
ASTM D790
Izod Impact, Notched 15.0 J/cm
28.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Shrinkage 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
ASTM D257
Surface Resistance 3.00e+14 ohm
3.00e+14 ohm
ASTM D257
Dielectric Constant 4.7
4.7
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Dissipation Factor 0.0090
0.0090
ASTM D150
Arc Resistance 134 sec
134 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 132 - 149 °C
270 - 300 °F
Mold temperature