Mechanical Properties Metric English Comments
Flexural Yield Strength 413 MPa
59900 psi
ASTM D790
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC  (discontinued **)
QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee..
Flexural Yield Strength 413 MPa
59900 psi
ASTM D790
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC  (discontinued **)
QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and ..
Flexural Yield Strength 413 MPa
59900 psi
ASTM D790
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC  (discontinued **)
QC-8704FR is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, an..