Radici Radiflam® S AE (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® S AE (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Water Absorption 7.2 %
7.2 %
Moisture Absorption at Equilibrium 2.1 %
2.1 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
Elongation at Break 12 %
12 %
Nominal
Elongation at Yield 3.3 %
3.3 %
Tensile Modulus 3.45 GPa
500 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm