Radici Radilon® CA HS (cond.) Nylon 66/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® CA HS (cond.) Nylon 66/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® CA is a range of polyamide 66/6 copolymers obtained through the polymerization of hexamethylendiamine, adipic acid and caprolactam.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 25 %
25 %
Tensile Modulus 1.45 GPa
210 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.410 J/cm²

@Temperature -30.0 °C
1.95 ft-lb/in²

@Temperature -22.0 °F
0.680 J/cm²

@Temperature 23.0 °C
3.24 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V