Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® CS can be used for blown film extrusion in general as well as being particularly suited for co-extrusion with PE because it improves the transparency and thermoformability of the film.Application: Co-extrusion of cast/blown film high transparencyInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Viscosity Measurement 230
230
cm³/g Viscosity Number; ISO 307
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 5271/2
Elongation at Break 4.1 %
4.1 %
ISO 5271/2
Tensile Modulus 2.80 GPa
406 ksi
ISO 5271/2
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 210 - 220 °C
410 - 428 °F
ISO 11357-1
Processing Properties Metric English Comments
Moisture Content <= 0.060 %
<= 0.060 %
ISO 960D
Users viewing this material also viewed the following: