Radici Radilon® S CP300 (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S CP300 (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
Water Absorption 7.3 %
7.3 %
Moisture Absorption at Equilibrium 2.1 %
2.1 %
Viscosity Measurement 140
140
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
Elongation at Break 13 %
13 %
Nominal
Elongation at Yield 3.5 %
3.5 %
Tensile Modulus 5.05 GPa
732 ksi
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
0.540 J/cm²

@Temperature 23.0 °C
2.57 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm