Radici Radilon® SHSX (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® SHSX (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastomer modified free conditioningInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527-1/2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/2
Elongation at Yield 4.0 %
4.0 %
ISO 524-1/2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-1/2
Flexural Strength 85.0 MPa
12300 psi
ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75/2Af
Vicat Softening Point 185 °C
365 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Users viewing this material also viewed the following: