Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Water Absorption 0.13 %
0.13 %
24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Melt Flow 4.0 - 8.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
4.0 - 8.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 91
91
ASTM D785
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 5.172 GPa
750.1 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
Unannealed; ASTM D648
Vicat Softening Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm

@Thickness 3.17 mm
450 kV/in

@Thickness 0.125 in
in air; ASTM D149
Arc Resistance 120 sec
120 sec
ASTM D495