Material Notes:
REPOL Polypropylene C080MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol C080MA is recommended for use in injection molding processes where high impact strength is required. It is an ideal material for making furniture & industrial products. Repol C080MA contains antistatic agent that reduces static charge build up on products.Features:Consistent processabilityGood stiffness-impact balanceGood surface glossLow static charge build up and reduced dust pick upInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50mm/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
50mm/min; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% secant; ASTM D790A
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648