Material Notes:
REPOL Polypropylene H100EY is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H100EY is recommended for use in TQ (Tubular water Quench) and Cast Film. It contains slip and antiblock additives. Repol H100EY is an ideal material for textile overwraps, packaging of readymade garments, snack food, grocery and general purpose packaging.Features:Consistent processabilityGood gloss and clarityHigh melt strengthInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50mm/min; ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.260 J/cm

@Temperature 23.0 °C
0.487 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648