Reltek BONDiT™ A-43 Bonding Agent, Primer and Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ A-43 Bonding Agent, Primer and Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties: Adhesion promoter for most thermoplastics, thermoset materials, elastomers, polyurethanes.Can be used on metals, glass and ceramicApplications: High functionality produces good bond strength in bonding difficult-to-bond substrates, such as polyethylene. Suitable for a wide range of vulcanizing elastomers as adhesion promoter to most substrates for a wide range of vulcanizing elastomers. Used as a primer for PU and TPU overmolding to a wide range of substrates. Higher bond strengths with less material use, but lower moisture resistance than A-3. Ambient cure 60 min or short thermal cure. Slight amber.
Physical Properties Metric English Comments
Specific Gravity 1.018 - 1.038 g/cc
1.018 - 1.038 g/cc
ASTM D1298
Viscosity Measurement 4.5 - 8.5
4.5 - 8.5
ASTM D445
Optical Properties Metric English Comments
Refractive Index 1.442 - 1.448
1.442 - 1.448
ASTM D1218
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min
0.500 - 1.00 hour
Ambient
5.00 min

@Temperature 150 °C
0.0833 hour

@Temperature 302 °F
15.0 min

@Temperature 75.0 °C
0.250 hour

@Temperature 167 °F
Descriptive Properties Value Comments
Color Clear with stray color
Users viewing this material also viewed the following: