Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1 to1 mix ratio by volume.TIGA 108 is an epoxy adhesive system that provides excellent bond strength to most substrates. Recommended for production bonding applications, this low viscosity formulation can be easily dispensed and mixed in convenient one to one mix ratios. TIGA 108 is a gap fill adhesive which forms water resistant bonds, therefore is ideal for bonding applications where substrates will be subjected to water or high humidity environments for long periods of time.Applications: This product bonds well to iron, aluminum, bronze, brass, wood concrete, ceramic materials and glass. It maintains a resistance not only to water, but oil and gasoline as well. Cures to smooth glass like finish.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Viscosity 19000 cP

@Temperature 25.0 °C
19000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 10 ohm-cm
10 ohm-cm
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
Dielectric Strength >= 16.5 kV/mm
>= 420 kV/in
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 8.00 - 12.0 min

@Temperature 25.0 °C
8.00 - 12.0 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear, black, or white