DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)  (discontinued **

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)  (discontinued **.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Water Absorption 4.5 %
4.5 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 1.3 %
1.3 %
Humidity Absorption; Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/-2
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
IEC 60695-11-10
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.4

@Frequency 1e+6 Hz
3.4

@Frequency 1e+6 Hz
IEC 60250
3.5

@Frequency 100 Hz
3.5

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0060

@Frequency 100 Hz
0.0060

@Frequency 100 Hz
IEC 60250
0.012

@Frequency 1e+6 Hz
0.012

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 425 V
425 V
IEC 60112
Descriptive Properties Value Comments
Flame Retardant Yes
Flame Retarding Agent Yes
Heat stabilized or stable to heat Yes
Injection molding Yes
With Fillers Yes
Users viewing this material also viewed the following: