Resirene Resirene® HF-555 General Purpose Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Resirene S.A. de C.V.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resirene Resirene® HF-555 General Purpose Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Very High FlowEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640External Lubrication AvailableApplications:Thin Wall ApplicationsInjectionHard to Fill MoldsDisposablesCosmetics CasesInformation provided by US distributor Calsak Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 200 °C
17 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Tensile Modulus 3.103 GPa
450.1 ksi
ASTM D638
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
0.5 in.; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 88 %
88 %
ASTM D1003