Mechanical Properties Metric English Comments
Tensile Strength at Break 33.8 MPa
4900 psi
2 in/min; ASTM D638
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade
Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 33.8 MPa
4900 psi
after 16 hours in 50°C water
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler
Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th..
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Techmer ES Plastiblend® ABS GN005
Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc.
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Techmer ES Plastiblend® ABS NAT
Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc.
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Techmer ES Plastiblend® ABS 92RK
Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Techmer ES Plastiblend® ABS LE BK
Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene
Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora..
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Chase Plastics CP Pryme® NN200STL (COND, 50% RH) Nylon 66, Super-Toughened, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 33.8 MPa
4900 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE)
Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household..
Tensile Strength at Break 33.8 MPa
4900 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE)
Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to..
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D412
3M Scotchcast™ 4 Electrical Insulating Resin
3M Scotchcast Electrical Insulating Resin 4 is a two-part, epoxy insulating and encapsulating resin. This resin, mixed in its unique two-part bag, generates its own heat to cure. Its compatibility w..
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Techmer ES Plastiblend® ABS 8008
Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc.
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D638
Resirene Resirene® HF-555 General Purpose Polystyrene
Features:Very High FlowEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640External Lubrication AvailableApplications:Thin Wall ApplicationsInjectionHard to Fill MoldsDisposablesCosmetics Cas..
Copyright © lookpolymers.com All Rights Reserved