Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D 792
Linear Mold Shrinkage, Flow 0.0044 - 0.0054 cm/cm

@Thickness 3.20 mm
0.0044 - 0.0054 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 63.0 MPa
9140 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 99 %
99 %
Type I, 50 mm/min; ASTM D 638
Elongation at Yield 4.0 %
4.0 %
Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2.86 GPa
415 ksi
50 mm/min; ASTM D 638
Flexural Yield Strength 99.0 MPa
14400 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.77 GPa
402 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.890 J/cm

@Temperature -30.0 °C
1.67 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
4.47 J/cm

@Temperature 23.0 °C
8.37 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Impact Test 63.0 J

@Temperature 23.0 °C
46.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 61.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 70.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C

@Thickness 3.20 mm
172 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 92.0 °C
198 °F
Rate B/50; ASTM D 1525