Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP COLORCOMP D1000FH PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP D1000FH PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP COLORCOMP* D1000FH is a compound based on Polycarbonate resin containing Unfilled Custom Color. Added features of this material include: Low Extractible.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption 0.300 %
0.300 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 2.39 GPa
347 ksi
50 mm/min; ASTM D638
Thermal Properties Metric English Comments
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af