Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir RT 461F Polystyrene High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ASTM C177 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® S 757 G Q43 White 36609 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® S KR2866C ASA / PC Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 165 N/L GPPS Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 486N HIPS Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 495N HIPS Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | |
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic HYTAC-FLXT is a unique material, combining the toughness and higher friction of FLX with improved release characteristic through PTFE impregnation. The result is a new, tough syntactic with just th.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr.. |
|||
Thermal Conductivity | 0.170 - 0.190 W/m-K | 1.18 - 1.32 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® 348 Q Transparent SAN Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |