SABIC Innovative Plastics LNP LUBRICOMP AL004 ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP AL004 ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* AL004 is a compound based on Acrylonitrile Butadiene Styrene resin containing Lubricants. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 2.15 GPa
312 ksi
50 mm/min; ASTM D638
Flexural Strength 62.0 MPa
8990 psi
ASTM D790
Flexural Modulus 2.17 GPa
315 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C

@Thickness 3.20 mm
169 °F

@Thickness 0.126 in
unannealed; ASTM D648