Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DFL-4036 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
5 mm/min; ISO 527
Elongation at Break 2.7 %
2.7 %
5 mm/min; ISO 527
Flexural Strength 163 MPa
23600 psi
2 mm/min; ISO 178
Flexural Modulus 6.90 GPa
1000 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.45
0.45
ASTM D3702 Modified
Coefficient of Friction, Static 0.41
0.41
ASTM D3702 Modified
K (wear) Factor 44.3 x 10-8 mm³/N-M
22.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
UL 94