SABIC Innovative Plastics LNP LUBRICOMP EX10404H PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP EX10404H PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* EX10404H is a compound based on Polyetherimide containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 216 MPa
31300 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.3 %
1.3 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 21.54 GPa
3124 ksi
5 mm/min; ASTM D638
Flexural Strength 283 MPa
41000 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 17.3 GPa
2510 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.560 J/cm
1.05 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.76 J/cm
8.92 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 213 °C

@Thickness 3.20 mm
415 °F

@Thickness 0.126 in
unannealed; ASTM D648