SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer (Asia Pacific)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 20% Glass Fiber Reinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Tensile Modulus 6.72 GPa
975 ksi
50 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 5.75 GPa
834 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.25 J/cm
9.84 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 161 °C

@Thickness 3.20 mm
322 °F

@Thickness 0.126 in
unannealed; ASTM D648