Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK642FR BK851 PBT
(Unverified Data**) Crastin® SK642FR BK851 is a black 15% glass fiber reinforced, flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Perf.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | |
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | |
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO GF25 CC 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 25% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
Polyram RamSter PF300G8 PBT, 40% Glass Fiber 40% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | Nominal Laminate |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS Fiber: AS7 GS, UD, 150 g/m2Information provided by HexCel |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC618P PBT/PET Alloy, Anti-microbial Applications: Gas equipment partsFeatures: Good anti-microbialWarpagelessFlame resistantInformation provided by Toyobo. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced POM-MD30Information provided by BARLOG plastics GmbH. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Density | 1.58 g/cc @Temperature 23.0 °C |
0.0571 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G25 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement. |
|||
Density | 1.58 - 1.62 g/cc | 0.0571 - 0.0585 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 224 Rigid PVC, Extrusion Various profiles |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | |
LATI Laticonther 75 GR/50 PBT, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | Dry as molded |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Density | 1.58 g/cc | 0.0571 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |