Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK (Asia Pacific)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing Bearing Grade. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 139 MPa
20200 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 11.03 GPa
1600 ksi
50 mm/min; ASTM D638
Flexural Strength 206 MPa
29900 psi
ASTM D790
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.80 J/cm
8.99 ft-lb/in
ASTM D4812
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702 Modified
Coefficient of Friction, Static 0.23
0.23
ASTM D3702 Modified
K (wear) Factor 24.2 x 10-8 mm³/N-M
12.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 290 °C

@Thickness 3.20 mm
554 °F

@Thickness 0.126 in
unannealed; ASTM D648