SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* ZP001XXP is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Time 86400 sec
0.0090 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 21.3 %
21.3 %
ASTM D638
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.47 GPa
358 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648