Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256-56 |
Rotuba 860MH 686.4 Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Shell Carilon® DB6F1G30 Polyketone, Flame-Retarded, Tracking-Resistant, Glass-Reinforced Injection Molding Grade
&n Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F1G30 is a flame-retarded, 15 percent glass-fiber-reinforced, injection molding grade with mecha.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM Data |
Dow Questra® QA805 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Izod Impact, Notched | 1.17 J/cm @Diameter 3.17 mm |
2.19 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 731G High Impact Polystyrene
(discontinued **) Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs .. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SEH80 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled FR-V1 80C UV improved |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA 12 (Asia Pacific) LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA LNP* LUBRICOMP* UFL36SXC is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 4002 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific) LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008 |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature -30.0 °C |
2.19 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature -30.0 °C |
2.19 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature -30.0 °C |
2.19 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 LNP THERMOCOMP* PF006S is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature -30.0 °C |
2.19 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N1050 PPE+HIPS (Asia Pacific) Noryl* N1050 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Bapolene® PP5052 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1420B Polycarbonate, 20% Glass Reinforced A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties, modified for good impact with increased dimensional stability and overall toughness. 1423B with UV sta.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.19 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.19 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | Approximation; ISO 180/1U |
Albis Plastics Tedur® L 9560 PPS, 50% Mineral High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.18 mm |
2.19 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |